Our advantages

  • Performance advantage

    Balance of Toughness and Rigidity

    Enhance Physical Properties

    Avoid Issues from Over-Lubrication

  • Cost advantage

    Extend Screw Life

  • Production advantage

    Enhance Plasticizing Speed and Production Efficiency

    Prolong Operating Time

    Improve Filler Dispersion

Frequently Asked Questions

  • High filler loading keeps biting you—what should you tweak first?

    +

    Start with how your additives work together. When CaCO3 is heavy, you want better dispersion and fewer friction hot spots. That means:

    · Use a polar polyester wax inside the melt (internal lube) to spread fillers evenly and cool down those hotspots.

    · Pair it with an external lube to keep surfaces smooth without over-slicking the melt.

    · Add a polyester homopolymer for toughness, without making the sheet “rubbery.”

    Goal: fewer white residues on rolls and screws, less charring, cleaner surfaces, and a faster line.

  • What’s special about polar polyester waxes here?

    +

    They’re the “good roommates” in PVC-more compatible, so they stay put. Result:

    · Better filler dispersion

    · Lower friction heat and fewer brown spots

    · Less oily surface and less migration

    Perfect for CaCO3-rich floor/wall lines that need both dispersion and screw life.

  • How do you balance lubrication without killing mechanics?

    +

    Split the jobs:

    · Internal: polar polyester wax (helps fusion and dispersion)

    · External: high-density oxidized PE wax (helps release and gloss)

    We found the sweet spot is the minimum effective dose. If you see mechanicals dip, bring in a polyester homopolymer to get toughness back.

Rallychem Chemicals will provide you with professional consulting services, PVC/CPVC customized solution services, wax additives, wax emulsions, micro polymers customized production services, welcome to contact us.

Contact Us
WhatsApp
WhatsApp QR Code

WhatsApp

Phone

For Inquiries Please Call

Rallychem Will Be Happy To Assist You!

Phone

+86 13456396233

Email
Back to Top
Submit Inquiry