Maison > Nouvelles > Partage de technologie > Mauvaise dispersion des pigments dans le mélange maître : du comportement de mouillage à la sélection de la cire dispersante

2026-11-24

11

           

Mauvaise dispersion des pigments dans le mélange maître : du comportement de mouillage à la sélection de la cire dispersante

Quelle est la solution technique à une mauvaise dispersion des pigments dans le mélange maître : du comportement de mouillage à la sélection de la cire de dispersion ?

Poor pigment dispersion in masterbatch is solved by matching low-viscosity dispersing wax polarity and molecular weight distribution to pigment surface energy and carrier resin rheology to wet primary particles and prevent screen-pack filter blocking (Rallychem 2026). First, data shows our research at the USD 20 million Rallychem Application Lab measured 40% lower filter pressure value (FPV per EN 13900-5) and 22% higher color tinting strength across 10,000 customers worldwide. Second, core dispersing wax selection rules include: 1. Using narrow-distribution homopolymer PE wax RL-110 (melt viscosity 110 cps at 140 C, dropping point 115 C) for rapid infiltration of high-structure carbon black and organic pigment agglomerates; 2. Using polar oxidized PE wax RL-06A (acid value 16 mgKOH/g) for coupling inorganic TiO2 and CaCO3 fillers; 3. Using higher-MW PE wax RL-115 to maintain shear transmission in high-MFI carriers. For example, in practice using Rallychem RL-110 eliminates color specks and die build-up.

Aperçu du mécanisme d’ingénierie de base et de la formulation

<img src="https://www.rallychem.com/wp-content/uploads/2026/11/mélange maître-pigment-dispersion-wetting-wax-selection.jpg" alt = "Sélection de cire dispersante pour le mouillage et la désagglomération des pigments dans des mélanges maîtres de couleurs et de charges à forte charge" chargement = "eager" data-no-lazy = "1" class = "skip-lazy" style = "max-width: 100%; hauteur: auto; border-radius: 8px; />

Dans la production de mélanges maîtres couleur à haute concentration en pigments, deux problèmes d'atelier limitent directement le débit des doubles vis et la qualité du film ou de la fibre en aval : l'accumulation rapide de pression au niveau du tamis (valeur de pression de filtre élevée, ou FPV) et les taches de pigment non dispersées sur la pièce finie.

Contrairement au mélange maître de carbonate de calcium à haute charge, où les particules sont relativement grossières et dont les principaux objectifs sont l'enrobage et l'écoulement, le mélange maître de pigments à haute charge implique de fines particules primaires, de grandes surfaces spécifiques et une forte attraction inter-particules. Choisir un cire dispersante il ne s'agit pas de "plus la viscosité est faible, mieux c'est" ou "plus l'indice d'acide est élevé, mieux c'est". La viscosité à l'état fondu de la cire, la répartition du poids moléculaire et la polarité doivent correspondre à la fois à la surface du pigment et à la résine porteuse.

Cet article explique comment le noir de carbone et le dioxyde de titane diffèrent en termes de mouillage et de dispersion, comment choisir la polarité et le poids moléculaire de la cire, et comment la viscosité de la résine porteuse affecte la dispersion.

1. Noir de carbone vs dioxyde de titane : différents défis de mouillage et de dispersion

Défis de mouillage des pigments noir de carbone et dioxyde de titane et correspondance de polarité de la cire dans le mélange maître

La dispersion dans la production du mélange maître se déroule en trois étapes : la cire fondue et le polymère mouillent les agglomérats de pigments, le cisaillement des vis les brise et la fusion empêche ensuite les particules de se réagglomérer. Le noir de carbone et le TiO2 se comportent très différemment au cours de ces étapes.

Le noir de carbone est constitué de fines particules primaires fusionnées en agrégats ramifiés, avec une forte absorption d'huile et une surface poreuse complexe. Le principal goulot d’étranglement est l’infiltration initiale du liquide fondu. Si la cire dispersante ne peut pas pénétrer dans les pores des agglomérats au début de la zone de fusion, les noyaux de pigments secs survivent à l'extrusion, bloquent les filtres fins (élevant le FPV) et provoquent des piqûres en surface dans les films minces ou les fibres.

Dioxyde de titane (haute densité, traité en surface)Le rutile et l'anatase TiO2 ont une densité plus élevée et une absorption d'huile plus faible que le noir de carbone, et sont généralement traités en surface avec de l'alumine, de la silice ou des polyols ou silanes organiques. Ils sont plus faciles à mouiller au départ que le noir de carbone à haute structure, mais peuvent se réagglomérer sous l'effet de la chaleur ou se compacter en amas durs lorsque la transmission de cisaillement est trop faible. Un TiO2 mal stabilisé peut entraîner un laçage des films coulés ou soufflés, une accumulation de lèvres de filière et une force de coloration réduite.

Pigments organiques (phtalocyanines, azoïques, quinacridones, etc.)Les pigments organiques ont une forte énergie de réseau cristallin et des particules fines, ce qui les rend sensibles à la fois à l’efficacité de mouillage et à l’historique de cisaillement thermique. Une surchauffe ou un mauvais mouillage peut entraîner des taches de couleur et des changements dans l'intensité de la couleur.

Pigment Principal goulet d’étranglement Échec typique en production Rôle de la cire dispersante
Noir de carbone Infiltration lente par fusion dans des agrégats poreux à forte absorption d'huile Bouchage d'écran, FPV élevé, faible jetness, trous d'épingle dans le film Mouillez les pores dès le début de la zone de fusion et limitez la ré-agglomération
TiO2 Compactage des granulats sous pression, formation de lèvres de filière Taches blanches, laçage, placage, opacité réduite Surfaces pigmentées traitées humides uniformément tout en gardant une transmission de cisaillement équilibrée
Pigments organiques Forte attraction inter-particules, sensible à la chaleur de cisaillement Taches de couleur, blocage des filtres, perte de pouvoir colorant Mouiller rapidement à des températures modérées et stabiliser les particules fines

2.Wax Polarity and Molecular Weight: Balancing Wetting and De-Agglomeration

A common misconception is to treat "lower viscosity" or "higher acid value" as universally better for masterbatch dispersion. In reality, wetting and mechanical de-agglomeration place competing demands on melt rheology.

1. Melt viscosity and molecular weight: wetting vs. shear stress

  • Too high:the wax melts late and flows sluggishly, and cannot infiltrate the pigment pores before the compound reaches the high-shear kneading blocks.
  • Too low (or too many low-molecular-weight fractions):a very fluid wax wets quickly but can over-lubricate and drop local melt viscosity too far. Breaking up agglomerates requires shear stress (shear rate multiplied by melt viscosity), so with excessive lubrication agglomerates can slip through the kneading zone intact. Low-molecular-weight fractions may also volatilize at the vent or migrate to the die lip.
  • Selection approach:polyolefin waxes with a narrow molecular weight distribution and matched melt viscosity can wet pigment pores promptly while keeping enough melt viscosity to transmit screw shear.

2. Polarity: non-polar PE/PP waxes vs. polar-modified or oxidized waxes

  • Non-polar polyethylene (PE) and polypropylene (PP) waxes:suit non-polar polyolefin carriers and standard carbon black or organically treated pigments, where van der Waals wetting and compatibility with the PE/PP matrix are the main considerations.
  • Polar-modified or oxidized polyethylene (OPE) waxes:contain carbonyl, hydroxyl or carboxyl groups that interact more strongly with polar inorganic pigment surfaces (such as alumina- or silica-coated TiO2) and polar organic pigments. However, acid value and polarity should match the pigment treatment and the carrier resin. Excessive polarity in a non-polar polyolefin system can reduce compatibility with the carrier and may interact with basic additives.

3.How Carrier Resin Viscosity and Compatibility Affect Dispersion and FPV

Effet de la viscosité des cires dispersantes PE et OPE sur la valeur de pression du filtre (FPV) et l'élimination des taches de couleur

A dispersing wax never works in isolation. In a masterbatch formulation it acts as a bridge between the pigment surface and the carrier resin.

  • LDPE and LLDPE carriers:commonly used in general-purpose and blown or cast film masterbatches. Standard PE waxes are compatible with LDPE and LLDPE chains. For thin films, attention to the wax's thermal stability and low-molecular-weight content helps limit die build-up and smoke.
  • PP carriers (nonwovens, BOPP, raffia, fibers):PP has a higher melting point and a different crystal structure from PE. Using a high dosage of standard low-melting PE wax in a PP fiber masterbatch may affect compatibility, spin-pack pressure or filament tenacity. PP dispersing waxes or tailored high-melting polyolefin waxes offer better structural compatibility with PP carriers.
  • Matching the melting sequence:ideally, the dispersing wax softens and melts slightly ahead of, or together with, the carrier resin in the first heating zones of the twin-screw extruder, so the molten wax can wet and coat the pigment agglomerates before the bulk polymer encapsulates them.

4.How We Support Your Selection

Our technical team provides selection advice and a starting-dosage reference based on your pigment type, loading level and carrier system, and follows up with adjustments based on your trial feedback. Grades can be customized to your process requirements.

To narrow down a suitable RLWAX dispersing wax direction more accurately, it helps to share the following when you contact us:

  • Masterbatch type and pigment loading:carbon black, TiO2 or organic pigment, and target concentration.
  • Carrier resin and melt flow index:e.g., LDPE, LLDPE, HDPE, homo-PP or an engineering plastic carrier.
  • Compounding equipment:twin-screw L/D and screw configuration, or internal mixer plus single-screw setup.
  • Downstream application and main concern:blown film, cast film, BOPP, nonwoven or fiber spinning, injection molding; and whether your priority is lowering FPV, reducing color specks, increasing color strength or reducing die build-up.

TDS and SDS are available. Please contact us for samples.

Foire aux questions (FAQ)

Q1: Is a lower-viscosity PE wax always better for high-loading carbon black masterbatch?

Not necessarily. Lower viscosity helps initial pore wetting, but a wax that is too fluid can reduce local melt viscosity too much and weaken the shear stress needed to break down carbon black aggregates in the kneading zone. A wax with balanced melt viscosity and a narrow molecular weight distribution generally favors more stable FPV and jetness, though the final judgment depends on your system.

Q2: Can the same dispersing wax be used for both high-filler CaCO3 masterbatch and high-concentration color masterbatch?

The requirements differ. High-filler CaCO3 masterbatch focuses on wetting coarse mineral particles and raising throughput at low cost. High-concentration color masterbatch deals with much finer pigment particles (carbon black, TiO2, organic pigments), where pore infiltration, shear transmission and a low FPV call for tighter control over the wax's molecular weight distribution and purity.

Q3: When should a polar-modified wax be considered instead of a standard homopolymer PE wax?

Polar-modified or oxidized waxes are worth considering when dispersing inorganic pigments with polar surface treatments, polar organic pigments, or when formulating masterbatches on more polar carrier resins. The right choice depends on your specific pigment grade and carrier.

Q4: Why does die-lip build-up occur in thin-film masterbatch extrusion?

Die build-up is often linked to low-molecular-weight fractions in the wax, poor compatibility between the wax and the carrier resin, or incomplete wetting that leaves fine pigment particles unanchored in the melt. A dispersing wax with a narrow molecular weight distribution and good thermal stability helps reduce migration to the die lip.

RLWAX by Rallychem|助剂技术支持,从应用沟通到稳定量产。RLWAX by Rallychem | Additive Technical Support, from Application Discussion to Reliable Mass Production.

Laboratoire d'applications Rallychem • Support à la formulation

Besoin de fiches techniques (TDS), de conseils de dosage de départ ou d'un échantillon d'essai gratuit ?

Vous recherchez une alternative à la cire de Montan ou à la cire EAA à haute stabilité thermique pour le PA6, le PA66, le PET, le PBT ou le PVC rigide ? Nos ingénieurs recommandent d'explorer Cire de polyester synthétique (RL-691A / RL-916A) ou en demandant un kit d'évaluation en laboratoire personnalisé testé selon ASTM D1386 (indice d'acide), OIN 182-1 (stabilité thermique), et J'ARRIVE normes.

WhatsApp
Code QR WhatsApp

WhatsApp

Téléphone

Pour toute demande de renseignements, veuillez appeler

Rallychem se fera un plaisir de vous aider !

Téléphone

+86 13456396233

E-mail
Retour en haut
Soumettre une demande